RIMS - Repository of Institute for Material Testing
Institute for Material Testing
    • English
    • Српски
    • Српски (Serbia)
  • English 
    • English
    • Serbian (Cyrillic)
    • Serbian (Latin)
  • Login
View Item 
  •   RIMS
  • Institut za ispitivanje materijala
  • Radovi istraživača / Researchers' publications
  • View Item
  •   RIMS
  • Institut za ispitivanje materijala
  • Radovi istraživača / Researchers' publications
  • View Item
JavaScript is disabled for your browser. Some features of this site may not work without it.

Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'

Thumbnail
2020
378.pdf (591.5Kb)
Authors
Međo, Bojan
Arsić, Miodrag
Mladenović, Mladen
Savić, Zoran
Grabulov, Vencislav
Radosavljević, Zoran
Rakin, Marko
Article (Published version)
Metadata
Show full item record
Abstract
Topic of this work is the integrity assessment of the pipeline section from hydropower plant Pirot. Crack-like defect size, maximum depth, is determined based on non-destructive evaluation - the largest crack depth is taken as the initial value for load carrying capacity estimation. Also, the crack dimensions (both length and depth) are varied. Limit pressure values are determined from 3D and 2D models of pipes with axial cracks on external surface. The influence of tensile loading on the load carrying capacity of the pipes with circumferential cracks is also examined. Integrity of pipes with both types of defects (axial and circumferential) is assessed through application of FAD diagrams.
Keywords:
pipeline / integrity assessment / finite element method / FAD diagram
Source:
Structural Integrity and Life, 2020, 20, 1, 82-86
Publisher:
  • Institut za ispitivanje materijala, Beograd
Funding / projects:
  • Ministry of Education, Science and Technological Development, Republic of Serbia, Grant no. 200135 (University of Belgrade, Faculty of Technology and Metallurgy) (RS-200135)
  • Ministry of Education, Science and Technological Development, Republic of Serbia, Grant no. 200012 (Istitute of Material Testing of Serbia - IMS, Belgrade) (RS-200012)

ISSN: 1451-3749

WoS: 000531008800014

Scopus: 2-s2.0-85092178486
[ Google Scholar ]
9
2
Handle
https://hdl.handle.net/21.15107/rcub_technorep_4567
URI
http://rims.institutims.rs/handle/123456789/381
Collections
  • Radovi istraživača / Researchers' publications
Institution/Community
Institut za ispitivanje materijala
TY  - JOUR
AU  - Međo, Bojan
AU  - Arsić, Miodrag
AU  - Mladenović, Mladen
AU  - Savić, Zoran
AU  - Grabulov, Vencislav
AU  - Radosavljević, Zoran
AU  - Rakin, Marko
PY  - 2020
UR  - http://rims.institutims.rs/handle/123456789/381
AB  - Topic of this work is the integrity assessment of the pipeline section from hydropower plant Pirot. Crack-like defect size, maximum depth, is determined based on non-destructive evaluation - the largest crack depth is taken as the initial value for load carrying capacity estimation. Also, the crack dimensions (both length and depth) are varied. Limit pressure values are determined from 3D and 2D models of pipes with axial cracks on external surface. The influence of tensile loading on the load carrying capacity of the pipes with circumferential cracks is also examined. Integrity of pipes with both types of defects (axial and circumferential) is assessed through application of FAD diagrams.
PB  - Institut za ispitivanje materijala, Beograd
T2  - Structural Integrity and Life
T1  - Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'
EP  - 86
IS  - 1
SP  - 82
VL  - 20
UR  - https://hdl.handle.net/21.15107/rcub_technorep_4567
ER  - 
@article{
author = "Međo, Bojan and Arsić, Miodrag and Mladenović, Mladen and Savić, Zoran and Grabulov, Vencislav and Radosavljević, Zoran and Rakin, Marko",
year = "2020",
abstract = "Topic of this work is the integrity assessment of the pipeline section from hydropower plant Pirot. Crack-like defect size, maximum depth, is determined based on non-destructive evaluation - the largest crack depth is taken as the initial value for load carrying capacity estimation. Also, the crack dimensions (both length and depth) are varied. Limit pressure values are determined from 3D and 2D models of pipes with axial cracks on external surface. The influence of tensile loading on the load carrying capacity of the pipes with circumferential cracks is also examined. Integrity of pipes with both types of defects (axial and circumferential) is assessed through application of FAD diagrams.",
publisher = "Institut za ispitivanje materijala, Beograd",
journal = "Structural Integrity and Life",
title = "Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'",
pages = "86-82",
number = "1",
volume = "20",
url = "https://hdl.handle.net/21.15107/rcub_technorep_4567"
}
Međo, B., Arsić, M., Mladenović, M., Savić, Z., Grabulov, V., Radosavljević, Z.,& Rakin, M.. (2020). Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'. in Structural Integrity and Life
Institut za ispitivanje materijala, Beograd., 20(1), 82-86.
https://hdl.handle.net/21.15107/rcub_technorep_4567
Međo B, Arsić M, Mladenović M, Savić Z, Grabulov V, Radosavljević Z, Rakin M. Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'. in Structural Integrity and Life. 2020;20(1):82-86.
https://hdl.handle.net/21.15107/rcub_technorep_4567 .
Međo, Bojan, Arsić, Miodrag, Mladenović, Mladen, Savić, Zoran, Grabulov, Vencislav, Radosavljević, Zoran, Rakin, Marko, "Influence of defects on limit loads and integrity of the pipeline at hydropower plant 'Pirot'" in Structural Integrity and Life, 20, no. 1 (2020):82-86,
https://hdl.handle.net/21.15107/rcub_technorep_4567 .

DSpace software copyright © 2002-2015  DuraSpace
About RIMS | Send Feedback

OpenAIRERCUB
 

 

All of DSpaceCommunitiesAuthorsTitlesSubjectsThis institutionAuthorsTitlesSubjects

Statistics

View Usage Statistics

DSpace software copyright © 2002-2015  DuraSpace
About RIMS | Send Feedback

OpenAIRERCUB