RIMS - Repository of Institute for Material Testing
Institute for Material Testing
    • English
    • Српски
    • Српски (Serbia)
  • English 
    • English
    • Serbian (Cyrillic)
    • Serbian (Latin)
  • Login
View Item 
  •   RIMS
  • Institut za ispitivanje materijala
  • Radovi istraživača / Researchers' publications
  • View Item
  •   RIMS
  • Institut za ispitivanje materijala
  • Radovi istraživača / Researchers' publications
  • View Item
JavaScript is disabled for your browser. Some features of this site may not work without it.

Izbor punjenih žica za navarivanje železničkih šina

Selection of the flux cored wires for repair welding of the rails

Thumbnail
2006
47.pdf (896.2Kb)
Authors
Popović, Olivera
Prokić-Cvetković, Radica
Grabulov, Vencislav
Odanović, Zoran
Article (Published version)
Metadata
Show full item record
Abstract
U savremenim uslovima eksploatacije, šine su izložene sve većim brzinama i osovinskim opterećenjima, pa se javljaju i sve veća eksploatacijska oštećenja. Dok je habanje šina značajno smanjeno uvođenjem u upotrebu odgovarajućih čelika i sredstava za podmazivanje, greške nastale usled kontaktnog zamora, tzv. RCF (rolling contact fatigue) greške, postaju sve veći problem na visoko opterećenim prugama. Reparatura oštećenih delova šina postupkom navarivanja je standardna metoda održavanja šina u svetu, a manjim delom kod nas, pa su razvijeni poluautomatski postupci koji su zamenili sporo ručno navarivanje obloženim elektrodama. U radu su prikazani rezultati primene nekih samozaštitnih punjenih žica i punjenih žica za rad u zaštiti CO2 gasa koji se koriste za navarivanje šina. Prikazano je kako vrsta dodatnog materijala utiče na raspodelu tvrdoće kroz presek spoja i makroskopski izgled navara. Dobijeni rezultati predstavljaju dobru osnovu za dalja ispitivanja u cilju određivanja eksploatacis...kog veka repariranih šina.

In modern railway exploitation, rails are exposed to a constant increase of speed and axles loads, which are causing increased exploitation damages. While wear has been reduced by introducing appropriate steel and lubricants rolling contact fatigue (RCF) defects have become more prominent on highly busy routes. Reparation of damaged rails by hard facing is standard method of maintenance in the world, but not in our country. Slowly manual processes are replaced by half-automatic welding processes. This paper describes behavior of some self-shielded flux cored wires and gas-shielded flux cored wires which are using for hard facing processes. Influence of the type of filler material on the hardness distribution and macroscopic view of deposit metal is also shown. These results should be used for further testing according to determination of remain life of repaired rails.
Keywords:
šina / samozaštitna punjena žica / punjena žica u zaštiti gasa / oštećenje / navarivanje / self-shielded flux cored wire / rail / hardfacing / gas-shielded flux cored wire / damage
Source:
Zavarivanje i zavarene konstrukcije, 2006, 51, 4, 131-139
Publisher:
  • DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd

ISSN: 0354-7965

[ Google Scholar ]
Handle
https://hdl.handle.net/21.15107/rcub_machinery_625
URI
http://rims.institutims.rs/handle/123456789/50
Collections
  • Radovi istraživača / Researchers' publications
Institution/Community
Institut za ispitivanje materijala
TY  - JOUR
AU  - Popović, Olivera
AU  - Prokić-Cvetković, Radica
AU  - Grabulov, Vencislav
AU  - Odanović, Zoran
PY  - 2006
UR  - http://rims.institutims.rs/handle/123456789/50
AB  - U savremenim uslovima eksploatacije, šine su izložene sve većim brzinama i osovinskim opterećenjima, pa se javljaju i sve veća eksploatacijska oštećenja. Dok je habanje šina značajno smanjeno uvođenjem u upotrebu odgovarajućih čelika i sredstava za podmazivanje, greške nastale usled kontaktnog zamora, tzv. RCF (rolling contact fatigue) greške, postaju sve veći problem na visoko opterećenim prugama. Reparatura oštećenih delova šina postupkom navarivanja je standardna metoda održavanja šina u svetu, a manjim delom kod nas, pa su razvijeni poluautomatski postupci koji su zamenili sporo ručno navarivanje obloženim elektrodama. U radu su prikazani rezultati primene nekih samozaštitnih punjenih žica i punjenih žica za rad u zaštiti CO2 gasa koji se koriste za navarivanje šina. Prikazano je kako vrsta dodatnog materijala utiče na raspodelu tvrdoće kroz presek spoja i makroskopski izgled navara. Dobijeni rezultati predstavljaju dobru osnovu za dalja ispitivanja u cilju određivanja eksploataciskog veka repariranih šina.
AB  - In modern railway exploitation, rails are exposed to a constant increase of speed and axles loads, which are causing increased exploitation damages. While wear has been reduced by introducing appropriate steel and lubricants rolling contact fatigue (RCF) defects have become more prominent on highly busy routes. Reparation of damaged rails by hard facing is standard method of maintenance in the world, but not in our country. Slowly manual processes are replaced by half-automatic welding processes. This paper describes behavior of some self-shielded flux cored wires and gas-shielded flux cored wires which are using for hard facing processes. Influence of the type of filler material on the hardness distribution and macroscopic view of deposit metal is also shown. These results should be used for further testing according to determination of remain life of repaired rails.
PB  - DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd
T2  - Zavarivanje i zavarene konstrukcije
T1  - Izbor punjenih žica za navarivanje železničkih šina
T1  - Selection of the flux cored wires for repair welding of the rails
EP  - 139
IS  - 4
SP  - 131
VL  - 51
UR  - https://hdl.handle.net/21.15107/rcub_machinery_625
ER  - 
@article{
author = "Popović, Olivera and Prokić-Cvetković, Radica and Grabulov, Vencislav and Odanović, Zoran",
year = "2006",
abstract = "U savremenim uslovima eksploatacije, šine su izložene sve većim brzinama i osovinskim opterećenjima, pa se javljaju i sve veća eksploatacijska oštećenja. Dok je habanje šina značajno smanjeno uvođenjem u upotrebu odgovarajućih čelika i sredstava za podmazivanje, greške nastale usled kontaktnog zamora, tzv. RCF (rolling contact fatigue) greške, postaju sve veći problem na visoko opterećenim prugama. Reparatura oštećenih delova šina postupkom navarivanja je standardna metoda održavanja šina u svetu, a manjim delom kod nas, pa su razvijeni poluautomatski postupci koji su zamenili sporo ručno navarivanje obloženim elektrodama. U radu su prikazani rezultati primene nekih samozaštitnih punjenih žica i punjenih žica za rad u zaštiti CO2 gasa koji se koriste za navarivanje šina. Prikazano je kako vrsta dodatnog materijala utiče na raspodelu tvrdoće kroz presek spoja i makroskopski izgled navara. Dobijeni rezultati predstavljaju dobru osnovu za dalja ispitivanja u cilju određivanja eksploataciskog veka repariranih šina., In modern railway exploitation, rails are exposed to a constant increase of speed and axles loads, which are causing increased exploitation damages. While wear has been reduced by introducing appropriate steel and lubricants rolling contact fatigue (RCF) defects have become more prominent on highly busy routes. Reparation of damaged rails by hard facing is standard method of maintenance in the world, but not in our country. Slowly manual processes are replaced by half-automatic welding processes. This paper describes behavior of some self-shielded flux cored wires and gas-shielded flux cored wires which are using for hard facing processes. Influence of the type of filler material on the hardness distribution and macroscopic view of deposit metal is also shown. These results should be used for further testing according to determination of remain life of repaired rails.",
publisher = "DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd",
journal = "Zavarivanje i zavarene konstrukcije",
title = "Izbor punjenih žica za navarivanje železničkih šina, Selection of the flux cored wires for repair welding of the rails",
pages = "139-131",
number = "4",
volume = "51",
url = "https://hdl.handle.net/21.15107/rcub_machinery_625"
}
Popović, O., Prokić-Cvetković, R., Grabulov, V.,& Odanović, Z.. (2006). Izbor punjenih žica za navarivanje železničkih šina. in Zavarivanje i zavarene konstrukcije
DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd., 51(4), 131-139.
https://hdl.handle.net/21.15107/rcub_machinery_625
Popović O, Prokić-Cvetković R, Grabulov V, Odanović Z. Izbor punjenih žica za navarivanje železničkih šina. in Zavarivanje i zavarene konstrukcije. 2006;51(4):131-139.
https://hdl.handle.net/21.15107/rcub_machinery_625 .
Popović, Olivera, Prokić-Cvetković, Radica, Grabulov, Vencislav, Odanović, Zoran, "Izbor punjenih žica za navarivanje železničkih šina" in Zavarivanje i zavarene konstrukcije, 51, no. 4 (2006):131-139,
https://hdl.handle.net/21.15107/rcub_machinery_625 .

DSpace software copyright © 2002-2015  DuraSpace
About RIMS | Send Feedback

OpenAIRERCUB
 

 

All of DSpaceCommunitiesAuthorsTitlesSubjectsThis institutionAuthorsTitlesSubjects

Statistics

View Usage Statistics

DSpace software copyright © 2002-2015  DuraSpace
About RIMS | Send Feedback

OpenAIRERCUB