Претраживање
Приказ резултата 1-10 од 40
Uticaj aditiva na razvoj mikrostrukture i svojstava korundnog vatrostalnog betona / Effects of additives on development of microstructure and properties of corundum based refractory concrete
(Udruženje inženjera građevinarstva, geotehnike, arhitekture i urbanista "Izgradnja", Beograd, 2008)
U ovom radu su prikazani rezultati ispitivanja korundnog vatrostalnog betona i njegovih varijacija sa (silikatnom prašinom i hemijskim vezivnim sredstvom - Litopix P-56), kao i uticaj pomenutih aditiva na svojstva finalnog ...
Proučavanje međudejstva anjonskih i katjonskih glina pri aktivaciji montmorilonita / Study of anionic and cationic clay interaction during activation of montmorillonite
(Udruženje inženjera građevinarstva, geotehnike, arhitekture i urbanista "Izgradnja", Beograd, 2008)
Istraživanja u okviru ovog rada su obuhvatila proučavanje mehanizma promena reoloških osobina minerala montmorilonita pri oplemenjavanju sa natrijum-karbonatom i magnezijum-hidroksi-karbonatom. Mehanizam promena reoloških ...
Ocena kvaliteta opekarskih sirovina sa juga Srbije / Quality evaluation of south Serbia raw clay materials
(Udruženje inženjera građevinarstva, geotehnike, arhitekture i urbanista "Izgradnja", Beograd, 2008)
U radu su prikazani rezultati istraživanja kvaliteta tri opekarske sirovine sa juga Srbije: sa ležišta kod Leskovca, sa ležišta kod Vlasotinaca i sa ležišta kod Male Plane. Istraživanja su obuhvatila hemijske, mineraloške, ...
Preparation of flish sediments and their application in brick products manufacturing
(Trans Tech Publications Ltd, Durnten-Zurich, 2004)
Flish sediments represent atypical raw materials: marls, marly shales and shales. This paper presents the results of laboratory tests of shales. The paper points out the similarities and differences in technological ...
Influence of mineralizers on mullite synthesis
(American Ceramic Society, 2006)
Investigation of the optimal parameters for repair welding of the coal mill in the fossil power station
(Welding in the World, 2008)
As a part of the coal fired power stations a coal milling plant is important, as it supplies a coal and air mixture for combustion in a power plant. Coal milling plant is involved in wearing process, since the raw coal is ...
Welded joints behaviour in service with special reference to pressure equipment
(Springer, Dordrecht, 2009)
Quality and structural integrity of welded pressure equipment are defined by The Pressure Equipment Directive (97/23/EC). The problem is complex, due to welded joint imperfections, matching effect, heterogeneity of ...
An analysis of the influence of weldment heterogeneity in ferrite-austenite welded structure
(Welding in the World, 2009)
An analysis of the influence of heterogeneity of the ferriteaustenite welded joint on its integrity has been performed. The Charpy specimens, with notch positioned in different regions of welded joint, have been tested ...
Static and impact crack properties of a high-strength steel welded joint
(Elsevier Sci Ltd, Oxford, 2007)
in order to gain the benefits of weldable high-strength steels in pressurized equipment applications, satisfactory toughness and crack properties of the welded joint, both in the weld metal and the heat-affected-zone (HAZ), ...
Influence of Si content and cooling rates on the size of SDAS and the latent heat released in Al-Si(5-11)-Cu1 alloys
(Proceedings - European Metallurgical Conference, EMC 2007, 2007)
The latent heat of solidification of any alloy depends on the chemistry and the microstructure developed during solidification process. Effects of chemistry on the release of the latent heat during solidification and ...